黑点混色
1 塑胶原料有分解
2 塑胶原料碎屑卡入柱塞和料筒间
3 塑胶原料受到污染或带进杂质
4 塑胶原料颗粒不均匀
5 模腔排气不良
变形
1 模具温度太高、冷却时间不够
2 制品壁厚厚薄悬殊
3 顶针推出位不当,制品受力不均匀
4 模腔不光滑,脱模不顺畅,摩擦力太
种类编辑
热塑弹性体:CPE POE PBE SBR SBS SEBS SIS TPE TPEE TPO TPR TPSIV TPU TPV TPX 硅胶
通用塑料:ABSABS高胶粉 ADPOLY AS(SAN) CA CAB EAA EVA GPPS HDPE HIPS LDPE LLDPE MBS MDPE MS MVLDPE(茂金属) PP
PVC
ABS塑胶材料
ABS塑胶材料
工程塑料:ABS/PA ABS/PC ABS/PMMA AES APPEEL ASA ASA/PC CAP COC COP CPVC DAP EBA ECTFE EPDM ETFE EMA EPS EVOH
EXACT FEP IXEF K(Q)胶隐藏 EFEP LCBR LCP M/PE/PP MABS MMBS PA/ABS PA/MXD6 PA1010 PA10T PA11 PA12 PA1212/PTFE
PA12/PTFE PA46 PA4T PA6 PA6/66 PA610 PA610/PTFE PA612 PA612/F/PTFE PA66 PA66/CF PA66/C/PTFE PA66/F/PTFE
PA66/PTFE PA6T PA9T PAE PAR PB-1 PBT PBT/ABS PBT/ASA PBT/F/PTFE PBT/PET PC XLPE PC/ABSPC/AES PC/C/PTFE PC/CF
PC/HIPS PC/PBT PC/PET PC/PS PC/PTFE PC/TPFE PCT PCTA PCTA/PCTGPCTG PE/PTFE PEEK PEI PES PET PETG PA4T PE蜡
PFA PF PMMA POMPOM/PTFE POP PPA PPE PPE/PA PPO PPO/PA PP-R PPS PP-B PPSU PSM PSU PTFE PVDF SEPS SMMA SOE SPS
SURLYN THV UCAR UHMWP